Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 45 cm³/g | 45 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 45 cm³/g | 45 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |