Polymer Property : Viscosity Test = 330 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 330 cm³/g
330 cm³/g
Viscosity Number; ISO 307, 1157, 1628
DSM Akulon® S245-C PA66
High Viscosity
Viscosity Test 330 cm³/g
330 cm³/g
DAM; ISO 307 1157 1628
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..