Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 300 cm³/g | 300 cm³/g | DAM; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |