Polymer Property : Viscosity Test = 3.0 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 1.0 - 3.0 cm³/g

@Temperature 50.0 °C
1.0 - 3.0 cm³/g

@Temperature 122 °F
Grade A
Kazanorgsintez Polyalkylbenzene Resin
Production Method: Polyalkylbenzene resin is the by-product of isopropyl benzene production. Application: Intended for national economic needs and Grade A is exportedInformation Provided by Kazanorg..