Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 239 cm³/g | 239 cm³/g | Viscosity number |
BASF Capron® B135QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |