Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 225 cm³/g | 225 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® B 40 E 000000 Nylon 6 PA 6 extrusion grade, standard grade of high viscosity with processing aid/lubricant, not nucleated. |
|||
Viscosity Test | 225 cm³/g | 225 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® B 40 F 000000 Nylon 6, Film Grade PA 6, Film grade, high viscosity, without additives or processing aids, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polya.. |
|||
Viscosity Test | 225 cm³/g | 225 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® B 40 FAM 000000 Nylon 6, Film Grade PA 6 film grade of high viscosity with high slip agent and lubricant content, not nucleatedApplication Examples: flat and blown film with good surface slip and smoothness - including in the freshly .. |
|||
Viscosity Test | 225 cm³/g | 225 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® B 40 FKA 000000 Nylon 6, Film Grade PA 6 film grade of high viscosity, nucleated and lubricated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion for PA/PE composite films |