Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity Test = 215 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 215 cm³/g
215 cm³/g
0.5% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 36 Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™
Viscosity Test 215 cm³/g
215 cm³/g
0.5% in 96% H2SO4; ISO 307
Azoty Tarnow™ Alphalon™ 40 Nylon 6
A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™