Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 214 cm³/g | 214 cm³/g | Viscosity Number |
DSM Akulon® F232-D Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Viscosity Test | 214 cm³/g | 214 cm³/g | Viscosity Number |
DSM Akulon® F232-DH Nylon 6 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |