Polymer Property : Viscosity Test = 185 cm³/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity Test 185 cm³/g
185 cm³/g
Viscosity Number
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 185 cm³/g
185 cm³/g
Viscosity Number
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Viscosity Test 185 cm³/g
185 cm³/g
Viscosity Number
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)  (discontinued **)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..