Polymer Property : Viscosity Test = 181 cm³/g
Polymer Property :
Viscosity Test =
181 cm³/g
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Viscosity Test
181
cm³/g
181
cm³/g
Viscosity Number; ISO 307, 1157, 1628
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity