Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 153 cm³/g | 153 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Viscosity Test | 153 cm³/g | 153 cm³/g | Viscosity Number |
Arkema Group Lacovyl® PE 1801 H PVC LACOVYL PE 1801 H is a vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of plastisols. It is suitable for a wide range of applications.* MAIN CHARACTERI.. |