Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 151 cm³/g | 151 cm³/g | Viscosity number |
BASF Ultramid® A27 EZ 01 PA66 (Dry) Ultramid A27 EZ 01 is a low viscosity, general purpose PA66 grade for compounding and extrusion of monofilaments. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC,.. |