Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 144 cm³/g | 144 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® A 30 H2.0 901510 Nylon 66 PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |
|||
Viscosity Test | 144 cm³/g | 144 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Viscosity Test | 144 cm³/g | 144 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Durethan® A 30 000000 Nylon 66 PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels |