Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 136 cm³/g | 136 cm³/g | Reduced viscosity, K value = 73; ISO 1628-2 |
SolVin 173GB Polyvinyl Chloride Emulsion Polymer Made by emulsion polymerization.
APPLICATIONS
Calendering : plasticized films and sheets
Extrusion : rigid or plasticized pipes and profiles
In most cases, SolVin 173GB resin is used in blends with .. |
|||
Viscosity Test | 136 cm³/g | 136 cm³/g | DAM; formic acid 90%; ISO 307 1157 1628 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |