Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 124 cm³/g | 124 cm³/g | Viscosity Number |
Arkema Group Lacovyl® GS 1300 PVC LACOVYL GS 1300 is a vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics : Viscosity index (ISO 1628-2):124 ml/g,(K value:70). Apparent density (ISO 60):0.49 g.. |