Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 69.0 - 116 cm³/g | 69.0 - 116 cm³/g | Average value: 97.9 cm³/g Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Viscosity Test | 61.0 - 116 cm³/g | 61.0 - 116 cm³/g | Average value: 96.0 cm³/g Grade Count:15 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |