Polymer Property : Viscosity Test = 1.16 cm³/g
Polymer Property :
Viscosity Test =
1.16 cm³/g
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Viscosity Test
1.16
-
1.24
cm³/g
1.16
-
1.24
cm³/g
Q/NHS501
Beijing Ranger Chem BLUESTAR® 1120 PBT
Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co.