Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 1.1 cm³/g @Temperature 30.0 °C |
1.1 cm³/g @Temperature 86.0 °F |
Inherent Viscosity in DMF Solution |
Kureha KF Polymer 1100 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |