Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.80 - 2.50 mm | 0.0709 - 0.0984 in | |
Iran Petrochemical (PCC) TPC - 121 HS Expandable Polystyrene TPC - 121 HSApplication: low density blocksInformation provided by Iran Petrochemical Commercial Co. |