Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 1.02 - 1.30 mm | 0.0402 - 0.0512 in | |
BASF Styropor® KF 262M EPS Description: Expandable polystyrene (EPS) with pentane as a blowing agent. For the production of expanded foam. Block having bulk densities of 12-30 kg/m3 and fire characteristics in conformity with.. |