Polymer Property : Bead Size = 0.850 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.360 - 0.850 mm
0.0142 - 0.0335 in
Carrington Laboratory Analytical Methods 2155
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Bead Size 0.350 - 0.850 mm
0.0138 - 0.0335 in
>97%, 2% max <0.35
BASF Styropor® BF 422 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 6 wt% pentane as the blowing agent. Styropor BF products are compatible with many anti-stat, mineral oil and color additiv..
Bead Size 0.420 - 0.850 mm
0.0165 - 0.0335 in
>97%, 2% max <0.425
BASF Styropor® BFL 422 EPS
Description: Modified expandable polystyrene (EPS) containing approximately 3.75 – 3.95 wt% pentane as the blowing agent. Styropor BFL products are compatible with many anti-stat, mineral oil and c..