Physical Properties | Metric | English | Comments |
---|---|---|---|
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-300H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SF-301H Expandable Polystyrene (EPS) FR Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-301 Expandable Polystyrene (EPS) High Expansion Typical Application : Large FloatInformation provided by Samsung Cheil Industries. |
|||
Bead Size | 0.720 - 0.960 mm | 0.0283 - 0.0378 in | JIS Z8801 |
Samsung Cheil Industries Starex® SG-302 Expandable Polystyrene (EPS) High Expansion Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries. |