Polymer Property : Bead Size = 0.0535 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SF-200H Expandable Polystyrene (EPS) FR
Characteristics: High Strength, High ExpansionTypical Application : InsulationInformation provided by Samsung Cheil Industries.
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SG-201 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.
Bead Size 0.960 - 1.36 mm
0.0378 - 0.0535 in
JIS Z8801
Samsung Cheil Industries Starex® SG-202 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large Float, Fish Box (Large)Information provided by Samsung Cheil Industries.