Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 8.49 g/10 min @Load 21.6 kg, Temperature 190 °C |
8.49 g/10 min @Load 47.6 lb, Temperature 374 °F |
|