Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 60 g/10 min @Load 21.6 kg, Temperature 240 °C |
60 g/10 min @Load 47.6 lb, Temperature 464 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PBT 1455 PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel.. |
|||
High Load Melt Index | 60 g/10 min @Load 21.6 kg, Temperature 190 °C |
60 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Meilian Chemical PE62071 RED MASTERBATCH RED 62071 is a red LDPE-based masterbatch containing 30% pigment, designed for use in polyolefin resins (PE and PP, etc.). Color Index No.: Red 48:1.Method of Usage: RED PE62071 is designated for ea.. |