Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 44 g/10 min @Load 21.6 kg, Temperature 275 °C |
44 g/10 min @Load 47.6 lb, Temperature 527 °F |
Calculated from Volume Flow Rate of 40 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Akulon® K240-HP Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
High Load Melt Index | 44 g/10 min @Load 21.6 kg, Temperature 190 °C |
44 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow FINGERPRINT™ DFDA-7510 NT Linear Low Density Polyethylene Resin FINGERPRINT™ DFDA-7510 NT resin is produced using UNIPOL™ process technology. It is intended for use in micro irrigation tube, durable hose and tube, profile extrusion, and injection molded fitti.. |
|||
High Load Melt Index | 44 g/10 min @Load 21.6 kg, Temperature 190 °C |
44 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDB-7441 NT 7 Linear Low Density Polyethylene Resin DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose .. |