Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 4.9 g/10 min @Load 21.6 kg, Temperature 235 °C |
4.9 g/10 min @Load 47.6 lb, Temperature 455 °F |
|
Arkema Group Cristamid® MS 1700 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,M,12-020Semi-aromatic polyamide (PASA) grade for injection molding.Transparency even thick. Outstanding thermal properties due to its high glass temperature. Good chemic.. |