Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 4.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PE 1313
(discontinued **) PRE-ELEC PE 1313 is a conductive thermoplastic compound based on PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 13.. |
|||
High Load Melt Index | 4.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem HB 0055 HDPE Blow Molding Polyethylene
(discontinued **) Applications: 200 liters L-ring drums. Information provided by Braskem |
|||
High Load Melt Index | 4.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
4.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |