Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 3.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
3.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |