Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® CP 1315
(discontinued **) PRE-ELEC CP 1315 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg |
25 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg |
25 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Lumicene® M 3410 EP HDPE Film, sheet FINACENE® M 3410 EP is a medium density metallocene based polyethylene resin. FINACENE® M 3410 EP is especially dedicated to film applications where a higher rigidity, good transparency and shrink.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg, Temperature 190 °C |
25 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDD-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg, Temperature 250 °C |
25 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2452/3 Polyphenylene Ether + Styrene-Butadiene Blend This grade, which contains a halogen-free flame-retardant, is especially resistant to heat deformation. Applications include: functional electrical parts (e.g. switches, transformer housings, defle.. |
|||
High Load Melt Index | 25 g/10 min @Load 21.6 kg |
25 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Finacene® BM359SG HDPE, blow molding
(Unverified Data**) FINACENE® BM359 SG has been especially designed for the manufacture of blow moulded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono.. |