Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 2.1 g/10 min @Load 21.6 kg |
2.1 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Finathene® 56020 HDPE, blow molding, sheet
(discontinued **) FINATHENE® 56020 S is a very high molecular weight high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 56020 S has been especially developed for t.. |