Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 180 g/10 min @Load 21.6 kg, Temperature 190 °C |
180 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |