Physical Properties Metric English Comments
High Load Melt Index 17.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
17.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl..