Polymer Property : High Load Melt Index = 16 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
High Load Melt Index 16 g/10 min
16 g/10 min
ASTM D1238
LyondellBasell Alathon® L5008 High Density Polyethylene
ApplicationsALATHON L 5008 is a high molecular weight high density polyethylene copolymer resin with broad and bimodal molecular weight distribution.Regulatory StatusWhen L 5008 is compounded with a..
High Load Melt Index 16 g/10 min

@Load 21.6 kg,
Temperature 190 °C
16 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri..
High Load Melt Index 16 g/10 min

@Load 21.6 kg,
Temperature 250 °C
16 g/10 min

@Load 47.6 lb,
Temperature 482 °F
BASF Luranyl® KR 2403 G2 Polyphenylene Ether + Styrene-Butadiene Blend, 10% Glass Fiber Reinforced
General-purpose grade with 10% glass fiber for parts requiring especially good resistance to heat deformation.Applications: auto parts, steering-column cladding and water meters.Data was collected b..
High Load Melt Index 16 g/10 min

@Load 21.6 kg
16 g/10 min

@Load 47.6 lb
ISO 1133
Total Lacqtene® 2002 TN 40 HDPE, blow molding, pipe, sheet  (discontinued **)
LACQTENE® 2002 TN 40 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer.Information provided provided by Total Petrochemicals.Total Petrochemic..