Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 14 g/10 min @Load 21.6 kg |
14 g/10 min @Load 47.6 lb |
ISO 1133 |
Total Finathene® 53140 HDPE, blow molding, sheet
(discontinued **) Finathene® 53140 is a high density polyethylene produced by the slurry loop low pressure polymerization process FINATHENE® 53140 has been especially developed for the manufacturing of blow molded .. |
|||
High Load Melt Index | 14 - 24 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 - 24 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 14 - 24 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 - 24 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 14 g/10 min @Load 21.6 kg |
14 g/10 min @Load 47.6 lb |
ISO 1133 |
SIDPEC EGYPTENE® HD 3802 FA HDPE Film Applications:General purpose thin film, trash bags, merchant bagsBlending partnerFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 10D neck height.Information provi.. |
|||
High Load Melt Index | 14 g/10 min @Load 21.6 kg |
14 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total HT 514 MDPE film Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process. Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of .. |
|||
High Load Melt Index | 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDC-6145 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6145 NT 7 provides good parison stability, which contribu.. |