Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 9.0 dynes/cm | 9.0 dynes/cm | Harmonic Mean - Polar |
Eastman Eastman Embrace Copolyester for Shrink Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |