Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 52 dynes/cm | 52 dynes/cm | 0.1%-20°C |
Solvay SUPRAGIL® GN 4-4’ Dihydroxydiphenyl Sulphonate Condensate Sodium Salt Description: Dispersant with binding properties.Identification: 4-4’ DIHYDROXYDIPHENYL SULPHONATE CONDENSATE SODIUM SALTRN CAS: 102958 – 53 – 2Solubility: Soluble in water. Insoluble .. |