Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 4.2 dynes/cm | 4.2 dynes/cm | 200 ppm, Light Phase: Heptane |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |
|||
Surface Tension | 4.2 dynes/cm | 4.2 dynes/cm | 200 ppm, Light Phase: Cyclohexane |
3M Novec™ FC-4432 Fluorosurfactant 3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga.. |