Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 3.0 dynes/cm | 3.0 dynes/cm | Harmonic Mean - Polar |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |