Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 21.5 dynes/cm | 21.5 dynes/cm | |
Dow Corning XIAMETER® PMCPPMX-200 10,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10,000CS. 100% active, 10,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Surface Tension | 21.5 dynes/cm | 21.5 dynes/cm | |
Dow Corning XIAMETER® PMCPPMX-200 12,500CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 12,500CS. 100% active, 12,500 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Surface Tension | 21.5 dynes/cm | 21.5 dynes/cm | |
Dow Corning XIAMETER® PMCPPMX-200 30,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 30,000CS. 100% active, 30,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Surface Tension | 21.5 dynes/cm | 21.5 dynes/cm | |
Dow Corning XIAMETER® PMCPPMX-200 60,000CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 60,000CS. 100% active, 60,000 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |