Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 14 dynes/cm | 14 dynes/cm | 25°C |
Solvay Specialty Polymers PERFLUOROSOLVâ„¢ PFS1 Perfluorinated Cleaning Solvent PERFLUOROSOLV PFS-1 is a low molecular weight perfluoropolyether solvent and diluent that perfroms well in many electronic and semiconductor cleaning functions, such as: pump cleaning, degreasing, d.. |
|||
Surface Tension | 14 dynes/cm | 14 dynes/cm | 25°C |
Asahi Glass ASAHIKLIN AK-225FPL Hydrochlorofluorocarbon Solvent AK-225FPL is a mixture of HCFC-225 and a fluorinated solvent. This blend was developed for those customers needing a solvent which is compatible with common plastics, such as polymethylmethacrylate,.. |