Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 90 Mesh | 90 Mesh | % through 200 mesh |
Struktol CALCIUM STEARATE High purity, non-wettable, calcium stearate powder manufactured with high quality stearic acid.STRUKTOL® Calcium Stearate is used by the rubber and plastic industries as an effective elastomer pr.. |