Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 8.0 - 12 Mesh | 8.0 - 12 Mesh | US Sieve |
Potters Industries A-Series A-205 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |
|||
Particle Mesh Size | 8.0 Mesh | 8.0 Mesh | typical |
ATI Wah Chang Hafnium Oxide, HfO2 A free flowing, coarse, tan powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |