Polymer Property : Particle Mesh Size = 60.0 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 60.0 Mesh
60.0 Mesh
5-40%
H.C. Starck Amperweld® 1701.39 K2 Chromium Carbide RIII
HS Number: 284990
Particle Mesh Size 60.0 Mesh
60.0 Mesh
5-40%
H.C. Starck Amperweld® 1701.39 K3 Chromium Carbide RIII
HS Number: 284990