Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 300 Mesh | 300 Mesh | 5% retained |
Imerys G-200 HP Feldspar G-200 HP Feldspar is a high potassium aluminum silicate ground to 200 mesh for ceramic applications. G-200 HP offers high potassium content and low iron oxide per unit of alumina.Information provide.. |