Polymer Property : Particle Mesh Size = 200 Mesh Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Mesh Size 100 - 200 Mesh
100 - 200 Mesh
0.0026
Gromax Melamine (Fine Grade)
China KInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 100 - 200 Mesh
100 - 200 Mesh
0.4865
Gromax Standard GB9567-97
China NInformation provided by Gromax Enterprises Corp.
Particle Mesh Size 100 - 200 Mesh
100 - 200 Mesh
0.373
Gromax Standard GB9567-97
China SInformation provided by Gromax Enterprises Corp.