Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 70 - 140 Mesh | 70 - 140 Mesh | |
Potters Industries Spheriglass® 2024 Solid Glass Spheres Description: Spheriglass® fine solid glass spheres are used as an additive for thermoplastic and thermosetting resin systems. Glass spheres give products many benefits such as:Low Uniform Shrinkage.. |
|||
Particle Mesh Size | 100 - 140 Mesh | 100 - 140 Mesh | US Sieve |
Potters Industries A-Series P-0060 Soda-Lime Silica Technical Quality Solid Glass Spheres Technical Quality, A-Series glass spheres are used to reduce particle size in coatings and inks. Glass Spheres used in oil well drilling improve lubrication and overall efficiencies of down hole oil.. |