Physical Properties | Metric | English | Comments |
---|---|---|---|
One Hour Half Life Temperature | 110 °C | 230 °F | |
Akzo Nobel Trigonox® C-50D-pd Peroxide Cure Agent Trigonox C-50D-pd is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Chemical Description: tert-Butyl peroxybenzoate, pow.. |
|||
One Hour Half Life Temperature | 110 °C | 230 °F | |
Akzo Nobel Trigonox® C-40B-pd Peroxide Cure Agent Trigonox C-40B-pd is a monofunctional peroxide which is used for the crosslinking of organic rubbers and silicone rubbers.Chemical Description: tert-Butyl peroxybenzoate, powder, 40% with inert fill.. |