Physical Properties | Metric | English | Comments |
---|---|---|---|
One Hour Half Life Temperature | 122 °C | 252 °F | |
Akzo Nobel Trigonox® C-C75 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Butyl peroxybenzoate, 75% solution in odorless mineral spiritsCAS Num.. |
|||
One Hour Half Life Temperature | 122 °C | 252 °F | |
Akzo Nobel Trigonox® C Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of pol.. |