Polymer Property : One Hour Half Life Temperature = 117 °C Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
One Hour Half Life Temperature 117 °C
243 °F
Akzo Nobel Trigonox® BPIC-C75 Polymerization Initiator
Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates. Trigonox BPIC-C75 may also be used as an initiator for curing unsaturated polyester and vinyles..